Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 800 MPa @Temperature 23.9 °C |
116000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D3039 |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Tensile Strength, Yield | >= 800 MPa @Thickness 65.0 mm |
>= 116000 psi @Thickness 2.56 in |
|
ThyssenKrupp N-A-XTRA® 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |
|||
Tensile Strength, Yield | >= 800 MPa @Thickness 65.0 mm |
>= 116000 psi @Thickness 2.56 in |
|
ThyssenKrupp N-A-XTRA® M 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |
|||
Tensile Strength, Yield | 800 MPa @Strain 0.200 % |
116000 psi @Strain 0.200 % |
hardened |
Wieland Simidur KF Plus PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |
|||
Tensile Strength, Yield | 800 MPa @Temperature 90.6 °C |
116000 psi @Temperature 195 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 800 MPa @Temperature 25.0 °C |
116000 psi @Temperature 77.0 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 800 MPa @Temperature 20.0 °C |
116000 psi @Temperature 68.0 °F |
Round bar 1" diameter, 310 HB |
EDRO #2 Prehardened 4130 Holder Block EDRO #2™ is a vacuum-degassed Chromium-Molybdenum-alloyed steel which is supplied in the hardened and tempered condition. EDRO #2™ is characterized by excellent machinability, good resistance to i.. |
|||
Tensile Strength, Yield | 800 MPa @Temperature 20.0 °C |
116000 psi @Temperature 68.0 °F |
Round bar 1" diameter, 310 HB |
EDRO #3 Prehardened Mold Quality P20 Alloy Steel EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with.. |
|||
Tensile Strength, Yield | 800 MPa @Strain 0.200 % |
116000 psi @Strain 0.200 % |
Double Age |
Crucible Compaction Metals P/M 625 Corrosion Resistant Alloy P/M 625 (chemically, UNS N06625) is produced by the Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing (HIP) and/or extrusion. The Crucible powder con.. |