Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 652 MPa @Strain 0.200 % |
94600 psi @Strain 0.200 % |
30% Cold Worked |
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |