Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 638 MPa @Temperature 232 °C |
92500 psi @Temperature 450 °F |
T300, Plain Weave; Fill Tension; Dry |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Fabric Form Fiber: T300-3KInformation provided by HexCel |