Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 610 MPa @Temperature 24.0 °C |
88500 psi @Temperature 75.2 °F |
|
Hexcel® HexPly® F263 Epoxy Resin, F3T584 Carbon Fabric Hexcel designation: F3T584-42"-F263; Fiber: T300 CelionInformation provided by HexCel |
|||
Tensile Strength, Yield | 610 MPa @Strain 0.200 %, Temperature 200 °C |
88500 psi @Strain 0.200 %, Temperature 392 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |