Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 61.0 MPa @Temperature 23.0 °C |
8850 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 61.0 MPa @Thickness 9.50 - 25.4 mm, Temperature 1093 °C |
8850 psi @Thickness 0.374 - 1.00 in, Temperature 1999 °F |
0.2% offset |
Haynes Hastelloy® S alloy, flat products Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | 61.0 MPa @Temperature 23.0 °C |
8850 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Zytel® FG408L NC010 is a general purpose, lubricated, impact modified polyamide 66 resin with superior toughness for injection molding applications. It has been developed for consideration into app.. |
|||
Tensile Strength, Yield | 61.0 MPa @Strain 0.200 %, Temperature 1000 °C |
8850 psi @Strain 0.200 %, Temperature 1830 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |