Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 570 MPa @Strain 1.00 % |
>= 82700 psi @Strain 1.00 % |
|
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re.. |
|||
Tensile Strength, Yield | >= 570 MPa @Strain 1.00 % |
>= 82700 psi @Strain 1.00 % |
|
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red.. |
|||
Tensile Strength, Yield | >= 570 MPa @Strain 0.200 %, Temperature 150 °C |
>= 82700 psi @Strain 0.200 %, Temperature 302 °F |
|
ThyssenKrupp N-A-XTRA® 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | >= 570 MPa @Strain 0.200 %, Temperature 300 °C |
>= 82700 psi @Strain 0.200 %, Temperature 572 °F |
|
ThyssenKrupp N-A-XTRA® 700 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | 570 MPa @Temperature 24.0 °C |
82700 psi @Temperature 75.2 °F |
|
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel |