Mechanical Properties Metric English Comments
Tensile Strength, Yield 530 MPa

@Strain 0.200 %,
Temperature 400 °C
76900 psi

@Strain 0.200 %,
Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4313 Martensitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Tensile Strength, Yield 530 MPa

@Strain 0.200 %
76900 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
Outokumpu 4501 Duplex Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Tensile Strength, Yield 530 MPa

@Strain 0.200 %
76900 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Yield >= 530 MPa

@Strain 0.200 %,
Temperature 100 °C
>= 76900 psi

@Strain 0.200 %,
Temperature 212 °F
ThyssenKrupp N-A-XTRA® 550 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield >= 530 MPa

@Strain 0.200 %,
Temperature 400 °C
>= 76900 psi

@Strain 0.200 %,
Temperature 752 °F
ThyssenKrupp N-A-XTRA® 700 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield >= 530 MPa

@Thickness >=65.0 mm
>= 76900 psi

@Thickness >=2.56 in
ThyssenKrupp N-A-XTRA® M 550 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield 530 MPa

@Strain 0.200 %,
Thickness 76.2 - 127 mm
76900 psi

@Strain 0.200 %,
Thickness 3.00 - 5.00 in
Typical Strength
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..
Tensile Strength, Yield 530 MPa

@Strain 0.100 %,
Temperature 600 °C
76900 psi

@Strain 0.100 %,
Temperature 1110 °F
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy