Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 460 MPa @Strain 0.200 % |
66700 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Tensile Strength, Yield | 460 MPa @Strain 0.200 % |
66700 psi @Strain 0.200 % |
hardened |
Wieland Porta Aurium PFM Alloy All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin.. |
|||
Tensile Strength, Yield | 460 MPa @Strain 0.200 % |
66700 psi @Strain 0.200 % |
hardened |
Wieland Porta Maximum PFM Alloy All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin.. |
|||
Tensile Strength, Yield | >= 460 MPa @Strain 0.200 %, Thickness 9.90 - 12.5 mm |
>= 66700 psi @Strain 0.200 %, Thickness 0.390 - 0.492 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m.. |
|||
Tensile Strength, Yield | >= 460 MPa @Strain 0.200 %, Thickness 25.0 - 50.0 mm |
>= 66700 psi @Strain 0.200 %, Thickness 0.984 - 1.97 in |
Temper T651; Standard EN 485-2 |
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m.. |
|||
Tensile Strength, Yield | 460 MPa @Strain 0.200 %, Thickness 300 - 400 mm |
66700 psi @Strain 0.200 %, Thickness 11.8 - 15.7 in |
long-transverse direction |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Tensile Strength, Yield | 460 MPa @Strain 0.200 %, Thickness 400 - 450 mm |
66700 psi @Strain 0.200 %, Thickness 15.7 - 17.7 in |
long-transverse direction |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Tensile Strength, Yield | 460 MPa @Strain 0.200 %, Thickness 150 - 240 mm |
66700 psi @Strain 0.200 %, Thickness 5.91 - 9.45 in |
Typical Strength |
Constellium Certal® SPC Aluminum Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man.. |
|||
Tensile Strength, Yield | 460 MPa @Strain 0.200 %, Thickness 325 - 400 mm |
66700 psi @Strain 0.200 %, Thickness 12.8 - 15.7 in |
Typical Strength |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |
|||
Tensile Strength, Yield | 460 MPa @Strain 0.200 %, Thickness 400 - 450 mm |
66700 psi @Strain 0.200 %, Thickness 15.7 - 17.7 in |
Typical Strength |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |
|||
Tensile Strength, Yield | >= 460 MPa @Strain 0.200 %, Thickness 7.90 - 12.5 mm |
>= 66700 psi @Strain 0.200 %, Thickness 0.311 - 0.492 in |
Temper T651 |
Constellium Certal® Thick Aluminum Plate Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and .. |
|||
Tensile Strength, Yield | >= 460 MPa @Strain 0.200 %, Thickness 12.5 - 25.0 mm |
>= 66700 psi @Strain 0.200 %, Thickness 0.492 - 0.984 in |
Temper T651 |
Constellium Certal® Thick Aluminum Plate Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and .. |
|||
Tensile Strength, Yield | >= 460 MPa @Strain 0.200 %, Thickness 25.0 - 50.0 mm |
>= 66700 psi @Strain 0.200 %, Thickness 0.984 - 1.97 in |
Temper T651 |
Constellium Certal® Thick Aluminum Plate Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and .. |
|||
Tensile Strength, Yield | 460 MPa @Strain 0.200 % |
66700 psi @Strain 0.200 % |
5% Cold Worked |
AK Steel 439 ULTRA FORM® Stainless Steel AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul.. |
|||
Tensile Strength, Yield | >= 460 MPa @Strain 0.200 % |
>= 66700 psi @Strain 0.200 % |
|
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34 Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion.. |