Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 458 MPa @Diameter 12.7 mm |
66400 psi @Diameter 0.500 in |
As welded; 0.2% offset |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Yield | 458 MPa @Thickness 12.7 mm, Temperature 93.0 °C |
66400 psi @Thickness 0.500 in, Temperature 199 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |