Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 414 MPa @Temperature 216 °C |
60000 psi @Temperature 420 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Tensile Strength, Yield | 414 MPa @Temperature 23.9 °C |
60000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Tensile Strength, Yield | 414 MPa @Temperature 216 °C |
60000 psi @Temperature 420 °F |
0° Direction, Dry, Autoclave with Post-Cure; ASTM D638 |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Tensile Strength, Yield | 414 MPa @Temperature 260 °C |
60000 psi @Temperature 500 °F |
0° Direction, Dry, Autoclave with Post-Cure; ASTM D638 |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Tensile Strength, Yield | 414 MPa @Temperature 71.1 °C |
60000 psi @Temperature 160 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Strength, Yield | 414 MPa @Temperature 23.9 °C |
60000 psi @Temperature 75.0 °F |
0° Direction, Dry; Autoclave, 50 psi, 90min; ASTM D638 |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |
|||
Tensile Strength, Yield | 414 MPa @Temperature 23.9 °C |
60000 psi @Temperature 75.0 °F |
0° Direction, Wet; ASTM D638 Type 1 |
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:.. |
|||
Tensile Strength, Yield | >= 414 MPa @Strain 0.200 %, Thickness 25.4 - 38.1 mm |
>= 60000 psi @Strain 0.200 %, Thickness 1.00 - 1.50 in |
ASTM E-8 |
H.C. Starck 3203 Pure Molybdenum APL, Arc-Cast, Low Carbon Plate Arc-Cast Plate 3203 Low CarbonDescription of Product: This specification covers rolled plate of carbon-deoxidized molybdenum produced from ingots consolidated by the H.C. Starck consumable electrod.. |
|||
Tensile Strength, Yield | >= 414 MPa @Diameter 47.63 - 73.03 mm, Strain 0.200 % |
>= 60000 psi @Diameter 1.875 - 2.875 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Pure Molybdenum AB, Arc-Cast Bar Arc-Cast BarDescription of Product: This specification covers carbon-deoxidized molybdenum wrought bar produced from ingots consolidated by the H.C. Stark consumable electrode vacuum-arc-casting pr.. |
|||
Tensile Strength, Yield | >= 414 MPa @Diameter 47.63 - 73.03 mm, Strain 0.200 % |
>= 60000 psi @Diameter 1.875 - 2.875 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Pure Molybdenum ABL, Arc-Cast, Low Carbon Bar Description of Product: This specification covers carbon-deoxidized, low-carbon molybdenum wrought bar produced from ingots consolidated by the H.C. Starck consumable electrode vacuum-arc-casting p.. |
|||
Tensile Strength, Yield | 414 MPa @Temperature 71.0 °C |
60000 psi @Temperature 160 °F |
1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F515; Fiber 75-1/0Information provided by HexCel |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 %, Thickness 127 - 152 mm |
60000 psi @Strain 0.200 %, Thickness 5.00 - 6.00 in |
Tension; Aquamet 22 HS |
Crucible Steel Aquamet® 22 Stainless Steel AQUAMET 22 is a high-alloy stainless steel with superior corrosion resistance along with excellent toughness and high strength. It has higher strength than AQUAMET 17 in 3/4" to 1-1/4" dia., and it .. |
|||
Tensile Strength, Yield | 414 MPa @Strain 0.200 % |
60000 psi @Strain 0.200 % |
18-20in thick |
Clinton Aluminum Alumold 1-500 Forged Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is .. |
|||
Tensile Strength, Yield | >= 414 MPa @Strain 0.500 %, Thickness <=25.4 mm |
>= 60000 psi @Strain 0.500 %, Thickness <=1.00 in |
|
Cadi 150 Copper Alloy A small addition of Zr to copper improves resistance to softening and resists deformation at high temperatures where normal copper would soften rapidly. Zirconium copper is used as a Class 1 electr.. |
|||
Tensile Strength, Yield | >= 414 MPa @Strain 0.500 %, Thickness <=25.4 mm |
>= 60000 psi @Strain 0.500 %, Thickness <=1.00 in |
|
Cadi 162 Copper Alloy Cadmium addition to copper increases hardness and resistance to softening. C16200 is utilized in numerous applications where fatigue strength and high electrical conductivity are required. Cadmium.. |
|||
Tensile Strength, Yield | 414 - 552 MPa @Strain 0.200 % |
60000 - 80000 psi @Strain 0.200 % |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |