Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 409 MPa @Strain 0.200 %, Thickness 12.7 mm |
59300 psi @Strain 0.200 %, Thickness 0.500 in |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |