Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 403 MPa @Thickness 1.70 mm, Temperature 204 °C |
58500 psi @Thickness 0.0669 in, Temperature 399 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |