Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 377 MPa @Thickness 12.7 mm, Temperature 371 °C |
54700 psi @Thickness 0.500 in, Temperature 700 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Tensile Strength, Yield | 377 MPa @Diameter 12.7 mm, Temperature 538 °C |
54700 psi @Diameter 0.500 in, Temperature 1000 °F |
0.2% offset |
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |