Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 354 MPa @Thickness 12.7 mm, Temperature 260 °C |
51300 psi @Thickness 0.500 in, Temperature 500 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Tensile Strength, Yield | 354 MPa @Strain 0.200 % |
51300 psi @Strain 0.200 % |
>0.05" |
AK Steel 430 ULTRA FORM® Stainless Steel 430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste.. |