Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 320 MPa @Strain 1.00 % |
46400 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 320 MPa @Strain 1.00 % |
46400 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 320 MPa @Strain 0.200 % |
46400 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 320 MPa @Strain 1.00 % |
46400 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 320 MPa @Strain 1.00 % |
46400 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 320 MPa @Strain 0.200 % |
46400 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 320 MPa @Strain 1.00 % |
46400 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 320 MPa @Strain 0.200 % |
46400 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4713 High Temperature Ferritic Stainless Steel Does not form brittle phases but should only be exposed to moderately corrosive atmospheres due to low chromium content.Applications: Mostly used in high temperature applications with sulphurous atm.. |
|||
Tensile Strength, Yield | >= 320 MPa @Strain 1.00 % |
>= 46400 psi @Strain 1.00 % |
|
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Tensile Strength, Yield | >= 320 MPa @Strain 0.200 % |
>= 46400 psi @Strain 0.200 % |
|
Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43 Description: URANUS® B26 (UR B26) is a 25% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed for high structural stability and high corr.. |
|||
Tensile Strength, Yield | >= 320 MPa @Strain 0.200 %, Thickness <=7.938 mm |
>= 46400 psi @Strain 0.200 %, Thickness <=0.3125 in |
per ASTM A240; transverse |
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |
|||
Tensile Strength, Yield | 320 MPa @Strain 0.200 % |
46400 psi @Strain 0.200 % |
Typical |
Aleris Weldural Aluminum Alloy, 300 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Tensile Strength, Yield | 320 MPa @Thickness 1.70 mm, Temperature 427 °C |
46400 psi @Thickness 0.0669 in, Temperature 801 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Tensile Strength, Yield | 320 MPa @Thickness 3.20 mm, Temperature 204 °C |
46400 psi @Thickness 0.126 in, Temperature 399 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Tensile Strength, Yield | 320 MPa @Strain 1.00 % |
46400 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 725LN Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Tensile Strength, Yield | 320 MPa @Strain 0.200 %, Temperature 250 °C |
46400 psi @Strain 0.200 %, Temperature 482 °F |
EN min.; EN 10002-5 |
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |