Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 319 MPa @Temperature 93.0 °C |
46300 psi @Temperature 199 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric Hexcel designation: 120-38"-F155; Fiber: 450-1/2Information provided by HexCel |
|||
Tensile Strength, Yield | 319 MPa @Strain 0.200 %, Temperature 93.0 °C |
46300 psi @Strain 0.200 %, Temperature 199 °F |
|
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Tensile Strength, Yield | 319 MPa @Thickness 25.4 mm, Temperature 25.0 °C |
46300 psi @Thickness 1.00 in, Temperature 77.0 °F |
0.2% Offset |
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |