Tensile Strength, Yield 303 - 359 MPa

@Strain 0.200 %
43900 - 52100 psi

@Strain 0.200 %
Typical
AK Steel 18 Cr-Cb™ Ferritic Stainless steel
AK Steel 18 Cr-Cb™ provides a more effective solution than Type 409 to many automotive exhaust applications, due to its higher oxidation resistance, improved creep resistance and moderate formabili..
Tensile Strength, Yield 303 - 372 MPa

@Strain 0.200 %,
Thickness 0.508 - 1.52 mm
43900 - 54000 psi

@Strain 0.200 %,
Thickness 0.0200 - 0.0600 in
ATI Allegheny Ludlum 430 Ferritic Stainless Steel
Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily..
Tensile Strength, Yield 303 MPa

@Thickness 3.20 mm,
Temperature 316 °C
43900 psi

@Thickness 0.126 in,
Temperature 601 °F
0.2% offset
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Tensile Strength, Yield 303 MPa

@Thickness 3.20 mm,
Temperature 427 °C
43900 psi

@Thickness 0.126 in,
Temperature 801 °F
0.2% offset
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Tensile Strength, Yield 303 MPa

@Strain 0.200 %,
Time 3.60e+6 sec
43900 psi

@Strain 0.200 %,
Time 1000 hour
Room Temperature properties after Isothermal Exposure
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy
INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar..
Tensile Strength, Yield 303 MPa

@Strain 0.200 %,
Treatment Temp. 760 °C
43900 psi

@Strain 0.200 %,
Treatment Temp. 1400 °F
Room Temperature properties after Isothermal Exposure
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy
INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar..