Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.92 MPa

@Strain 5.00 %
569 psi

@Strain 5.00 %
ASTM D638
SK Chemicals SKYPEL P147D Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Yield 3.92 MPa

@Strain 300 %
569 psi

@Strain 300 %
ASTM D412
SK Chemicals SKYTHANE® 850A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 3.92 MPa

@Strain 5.00 %
569 psi

@Strain 5.00 %
ASTM D638
Samyang Triel® 5401BM Thermoplastics Polyetherester Elastomer, Blow Molding
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5401BM is for blow molding applications.Applications: Automotive - CVJB and BellowsInformation provided ..
Tensile Strength, Yield 3.92 MPa

@Strain 5.00 %
569 psi

@Strain 5.00 %
ASTM D638
Samyang Triel® 5501BM Thermoplastics Polyetherester Elastomer, Blow Molding
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5501BM is for blow molding applications.Applications: Automotive BellowsInformation provided by Samyang...
Tensile Strength, Yield 3.92 MPa

@Strain 10.0 %
569 psi

@Strain 10.0 %
ASTM D638
SK Chemicals SKYPEL P137DW Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Yield 3.92 MPa

@Strain 300 %
569 psi

@Strain 300 %
ASTM D412
SK Chemicals SKYTHANE® 410 Hotmelt Grade UB Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 3.92 MPa

@Strain 100 %
569 psi

@Strain 100 %
ASTM D412
SK Chemicals SKYTHANE® 420 Hotmelt Grade UB Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 3.92 MPa

@Strain 100 %
569 psi

@Strain 100 %
ASTM D412
SK Chemicals SKYTHANE® 470A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 3.92 MPa

@Strain 100 %
569 psi

@Strain 100 %
ASTM D412
SK Chemicals SKYTHANE® 385A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..