Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.90 MPa

@Strain 10.0 %
566 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® EM402-L Polyether Ester Elastomer (European Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 3.90 MPa

@Strain 50.0 %
566 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 2058A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..
Tensile Strength, Yield 3.90 MPa

@Strain 50.0 %
566 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 5085A Polyether TPU Resin
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro..
Tensile Strength, Yield 3.90 MPa

@Strain 10.0 %
566 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 3.90 MPa

@Strain 10.0 %
566 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® EM400 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 3.90 MPa

@Strain 5.00 %
566 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 3.90 MPa

@Strain 5.00 %
566 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® EM460 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 3.90 MPa

@Strain 10.0 %
566 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® EM402-L Injection Molding; Coating Grade Copolyester Elastomer (North America)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Copyright © lookpolymers.com All Rights Reserved