Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.10 MPa @Strain 50.0 % |
450 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 1185A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 3.10 MPa @Strain 50.0 % |
450 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 1075A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 3.10 MPa @Strain 5.00 % |
450 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® PL420-H Injection Molding Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 3.10 MPa @Strain 5.00 % |
450 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® PL420-H Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 3.10 MPa @Strain 100 % |
450 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |