Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 270 MPa @Strain 1.00 %, Temperature 100 °C |
39200 psi @Strain 1.00 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 270 MPa @Strain 0.200 %, Temperature -80.0 °C |
39200 psi @Strain 0.200 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 270 MPa @Strain 0.200 % |
39200 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 270 MPa @Strain 0.200 % |
39200 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 270 MPa @Strain 0.200 % |
39200 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4439 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms. |
|||
Tensile Strength, Yield | 270 MPa @Strain 1.00 %, Temperature 300 °C |
39200 psi @Strain 1.00 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4565 High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 270 MPa @Strain 0.200 %, Temperature 200 °C |
39200 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4565 High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 270 MPa @Strain 0.200 % |
39200 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Tensile Strength, Yield | 270 MPa @Strain 0.200 % |
39200 psi @Strain 0.200 % |
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1 |
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Tensile Strength, Yield | 270 MPa @Strain 0.200 % |
39200 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Tensile Strength, Yield | 270 MPa @Strain 0.200 % |
39200 psi @Strain 0.200 % |
Typical |
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel CLC 17-12-2Ti is a Titanium stabilized austenitic stainless steel. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized co.. |
|||
Tensile Strength, Yield | >= 270 MPa @Strain 0.200 % |
>= 39200 psi @Strain 0.200 % |
|
Industeel CLC 18.10 LN Nitrogen Containing 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18.10LN is a 18Cr-10Ni austenitic stainless steel with specific Nitrogen additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior .. |
|||
Tensile Strength, Yield | 270 MPa @Thickness 9.50 mm, Temperature 316 °C |
39200 psi @Thickness 0.374 in, Temperature 601 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Tensile Strength, Yield | >= 270 MPa @Strain 2.00 % |
>= 39200 psi @Strain 2.00 % |
bake hardening after 2% strain and heating to 170°C for 20 min. |
SSAB Tunnplat Docol® 220 BH High-strength Steel High-strength SteelComments: Docol BH - Cold Rolled Steel - rephosphorized steel with bake hardening effect. Property values are for cold-rolled steel; thicknesses 0.40 - 2.0 mm. Iron content is ap.. |
|||
Tensile Strength, Yield | 270 MPa @Strain 0.200 %, Thickness 7.90 - 25.0 mm |
39200 psi @Strain 0.200 %, Thickness 0.311 - 0.984 in |
Typical Strength; Standard EN 485-2 |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |
|||
Tensile Strength, Yield | >= 270 MPa @Strain 0.200 %, Thickness 203.2 - 254 mm |
>= 39200 psi @Strain 0.200 %, Thickness 8.000 - 10.0 in |
Tempers T851/T852 |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Tensile Strength, Yield | >= 270 MPa @Strain 0.200 % |
>= 39200 psi @Strain 0.200 % |
Minimum |
Aleris Weldural Aluminum Alloy, 200 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |