Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2648 MPa @Temperature 23.0 °C |
384100 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, T5A120 Carbon Tape Hexcel designation: TXX120-12"-F515; Fiber: IM6Information provided by HexCel |