Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 262 MPa @Temperature 23.9 °C |
38000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® F-562 Phenolic Prepreg, C2 Carbonized Rayon Reinforced Nelcote® F-562 is an elastomer modified phenolic resin used in the manufacture of intermediate temperature ablative rocket nozzles, heat shields and combustion chambers in highly oxidative environm.. |
|||
Tensile Strength, Yield | 262 MPa @Thickness 1.57 mm |
38000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP130 Glass Fabric Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic.. |
|||
Tensile Strength, Yield | 262 MPa @Thickness 23.4 mm, Temperature 400 °C |
38000 psi @Thickness 0.921 in, Temperature 752 °F |
0.2% offset |
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 262 MPa @Thickness 46.1 mm, Temperature 400 °C |
38000 psi @Thickness 1.81 in, Temperature 752 °F |
0.2% offset |
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | >= 262 MPa @Strain 0.200 % |
>= 38000 psi @Strain 0.200 % |
Specification |
AK Steel 18 Cr-Cb™ Ferritic Stainless steel AK Steel 18 Cr-Cb™ provides a more effective solution than Type 409 to many automotive exhaust applications, due to its higher oxidation resistance, improved creep resistance and moderate formabili.. |
|||
Tensile Strength, Yield | 262 MPa @Strain 0.200 %, Temperature 400 °C |
38000 psi @Strain 0.200 %, Temperature 752 °F |
Typical annealed sample; short time elevated temp. |
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |
|||
Tensile Strength, Yield | 262 MPa @Temperature 204 °C |
38000 psi @Temperature 399 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 705 Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other .. |