Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 24.0 MPa @Strain 300 % |
3480 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1055DE Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp.. |
|||
Tensile Strength, Yield | 24.0 MPa @Strain 300 % |
3480 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1095AF Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject.. |
|||
Tensile Strength, Yield | 24.0 MPa @Strain 300 % |
3480 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 3095A Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength, Yield | 24.0 MPa @Strain 300 % |
3480 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1095A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 24.0 MPa @Temperature 121 °C |
3480 psi @Temperature 250 °F |
ASTM D638 |
BASF Ultramid® 8270 HS BK 102 PA6 (Dry) Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex.. |
|||
Tensile Strength, Yield | 24.0 MPa @Strain 100 % |
3480 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® C-60D Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fue.. |
|||
Tensile Strength, Yield | 24.0 MPa @Strain 100 % |
3480 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® UM551 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 24.0 MPa @Strain 100 % |
3480 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® UM551 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |