Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 239 MPa @Strain 0.200 %, Temperature 650 °C |
34700 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |