Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 215 MPa @Strain 1.00 %, Temperature 200 °C |
31200 psi @Strain 1.00 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Yield | 215 MPa @Strain 1.00 %, Temperature 200 °C |
31200 psi @Strain 1.00 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Tensile Strength, Yield | >= 215 MPa @Strain 0.200 % |
>= 31200 psi @Strain 0.200 % |
|
Industeel URANUS® 65 310 L Modified Grade - Low C and Si for Nitric Acid Service Description: URANUS® 65 is a 25 Cr 20 Ni austenitic stainless steel with sharp control of the residual elements in order to provide high corrosion resistance properties in boiling 50-65% Nitric a.. |
|||
Tensile Strength, Yield | 215 MPa @Strain 0.200 %, Temperature 427 °C |
31200 psi @Strain 0.200 %, Temperature 801 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Tensile Strength, Yield | 215 MPa @Strain 0.200 %, Temperature 427 °C |
31200 psi @Strain 0.200 %, Temperature 801 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |