Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 201 MPa @Strain 1.00 %, Temperature 100 °C |
29200 psi @Strain 1.00 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |