Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 190 MPa @Strain 1.00 %, Temperature 400 °C |
27600 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Yield | 190 MPa @Strain 0.200 %, Temperature 200 °C |
27600 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 190 MPa @Strain 1.00 %, Temperature 400 °C |
27600 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 190 MPa @Strain 0.200 %, Temperature 200 °C |
27600 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro.. |
|||
Tensile Strength, Yield | 190 MPa @Temperature 316 °C |
27600 psi @Temperature 601 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 705 Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other .. |
|||
Tensile Strength, Yield | 190 MPa @Temperature 23.0 °C |
27600 psi @Temperature 73.4 °F |
50 mm/min; ISO 527-1/-2 |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |