Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 19.0 MPa @Strain 10.0 % |
2760 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® UM622 General Purpose Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 19.0 MPa @Strain 10.0 % |
2760 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® UM622 Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 19.0 MPa @Strain 100 % |
2760 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 1055D Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 19.0 MPa @Strain 100 % |
2760 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 3065D Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength, Yield | 19.0 MPa @Strain 50.0 % |
2760 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 1065D Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 19.0 MPa @Strain 100 % |
2760 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 1160D Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 19.0 MPa @Temperature 23.0 °C |
2760 psi @Temperature 73.4 °F |
90° |
Hexcel® HexPly® 954-6 Curing Cyanate Resin, K13C-2U Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 19.0 MPa @Strain 100 % |
2760 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® S98A Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv.. |
|||
Tensile Strength, Yield | 19.0 MPa @Strain 300 % |
2760 psi @Strain 300 % |
0.76 mm (0.030 in) extruded sheet; ASTM D-412 |
BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tensile Strength, Yield | 19.0 MPa @Strain 300 % |
2760 psi @Strain 300 % |
0.76 mm (0.030 in) extruded sheet; ASTM D-412 |
BASF Elastollan® 1185A10U Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tensile Strength, Yield | 19.0 MPa @Strain 300 % |
2760 psi @Strain 300 % |
0.76 mm (0.030 in) extruded sheet; ASTM D-412 |
BASF Elastollan® 1185A10V Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |