Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 17.0 MPa @Temperature 121 °C |
2470 psi @Temperature 250 °F |
50%RH; ASTM D638 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 300 % |
2470 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1195A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 100 % |
2470 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 3055D Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 300 % |
2470 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 3090AF Polyether TPU Resin ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro.. |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 300 % |
2470 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 5090A Polyether TPU Resin ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro.. |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 100 % |
2470 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 1170D Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 100 % |
2470 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® PM460 General Purpose Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 100 % |
2470 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® PM460 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 50.0 % |
2470 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® PM581 58 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 50.0 % |
2470 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® PM581 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |