Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 162 MPa @Strain 1.00 %, Temperature 400 °C |
23500 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |
|||
Tensile Strength, Yield | 162 MPa @Strain 0.200 %, Temperature 100 °C |
23500 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |
|||
Tensile Strength, Yield | 162 MPa @Temperature 871 °C |
23500 psi @Temperature 1600 °F |
Vacuum |
ATI Wah Chang Nb/Nb Alloy C-103 This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig.. |