Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 1415 MPa @Strain 0.200 % |
>= 205200 psi @Strain 0.200 % |
H950 Condition - 500°C |
Latrobe Lescalloy® 13-8 Mo VIM-VAR Precipitation Hardening Stainless Steel Lescalloy 13-8 Mo VIM-VAR is a precipitation hardening martensitic stainless steel offering excellent fracture toughness and transverse mechanical properties coupled with the resistance to stress-co.. |
|||
Tensile Strength, Yield | 1415 MPa @Strain 0.200 % |
205200 psi @Strain 0.200 % |
Cold Worked 48% |
Latrobe MP159® Alloy MP159 is an alloy of the Multiphase family of alloys possessing the unique combination of ultra-high strength, ductility and corrosion resistance. Through work strengthening and aging, MP159 alloy .. |