Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 132 MPa @Strain 0.200 %, Temperature 300 °C |
19100 psi @Strain 0.200 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |
|||
Tensile Strength, Yield | 132 MPa @Temperature 982 °C, Time 11500 sec |
19100 psi @Temperature 1800 °F, Time 3.20 hour |
As Welded, Solution Annealed, and Aged; Base/Weld Fracture; 0.2% Offset |
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |