Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 128 MPa @Strain 1.00 %, Temperature 500 °C |
18600 psi @Strain 1.00 %, Temperature 932 °F |
EN min.; EN 10002-5 |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 128 MPa @Strain 0.200 %, Temperature 500 °C |
18600 psi @Strain 0.200 %, Temperature 932 °F |
EN min.; EN 10002-5 |
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 128 MPa @Strain 1.00 %, Temperature 500 °C |
18600 psi @Strain 1.00 %, Temperature 932 °F |
EN min.; EN 10002-5 |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 128 MPa @Strain 1.00 %, Temperature 500 °C |
18600 psi @Strain 1.00 %, Temperature 932 °F |
EN min.; EN 10002-5 |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | >= 128 MPa @Temperature 20.0 °C |
>= 18600 psi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Tensile Strength, Yield | 128 MPa @Temperature 260 °C |
18600 psi @Temperature 500 °F |
short term exposure |
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us.. |
|||
Tensile Strength, Yield | 128 MPa @Temperature 871 °C |
18600 psi @Temperature 1600 °F |
ASTM E8 |
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Yield | 128 MPa @Thickness 1.57 mm |
18500 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP321 Cotton Fabric
(discontinued **) Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f.. |