Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1265 MPa @Strain 0.200 % |
183500 psi @Strain 0.200 % |
24°C Test Temp; 843°C Hardening Temp |
Latrobe CBS-600™ VIM-VAR Carburizing Bearing and Gear Steel CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe.. |