Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 11.3 MPa @Strain 10.0 % |
1640 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® PL471 45 Shore D, Injection Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 11.3 MPa @Strain 10.0 % |
1640 psi @Strain 10.0 % |
ASTM D638 |
SK Chemicals SKYPEL M555DH General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tensile Strength, Yield | 11.3 MPa @Strain 10.0 % |
1640 psi @Strain 10.0 % |
ASTM D638 |
SK Chemicals SKYPEL G455D Special Grade Oil-Resistant Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tensile Strength, Yield | 11.3 MPa @Strain 5.00 % |
1640 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® PB582-H 58 Shore D, Blow Molding Grade, Heat Stabilized Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 11.3 MPa @Strain 5.00 % |
1640 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® PB582-H Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 11.3 MPa @Strain 50.0 % |
1640 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® EB464 42 Shore D, Blow Molding Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 11.3 MPa @Strain 50.0 % |
1640 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® EB464 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 11.3 MPa @Strain 10.0 % |
1640 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® PL471 Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |