Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : K (wear) Factor = 15.9 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 9.00 - 32.0 x 10-8 mm³/N-M
4.47 - 15.9 x 10-10 in³-min/ft-lb-hr
Average value: 16.4 x 10<sup>-8</sup> mm³/N-M Grade Count:4
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..