Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 20.0 - 30.0 x 10-8 mm³/N-M | 9.93 - 14.9 x 10-10 in³-min/ft-lb-hr | at PV 100; ASTM D3702 |
Guarniflon PTFE G420 Polytetrafluoroethylene 50% Steel PTFE G Special Compound with steelInformation provided by Guarniflon® |
|||
K (wear) Factor | 20.0 - 30.0 x 10-8 mm³/N-M | 9.93 - 14.9 x 10-10 in³-min/ft-lb-hr | at PV 100; ASTM D3702 |
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w.. |
|||
K (wear) Factor | 20.0 - 30.0 x 10-8 mm³/N-M | 9.93 - 14.9 x 10-10 in³-min/ft-lb-hr | at PV 100; ASTM D3702 |
Guarniflon PTFE G415 Polytetrafluoroethylene 25% Soft Carbon PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high .. |