Mechanical Properties Metric English Comments
K (wear) Factor 111 x 10-8 mm³/N-M
55.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC
LNP LUBRICOMP* DL0029E is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant.
K (wear) Factor 111 x 10-8 mm³/N-M
55.0 x 10-10 in³-min/ft-lb-hr
40psi, 50ft/min; tested in accordance with LNP WI-0687
LNP Thermocomp® LC-1006 Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
K (wear) Factor 111 x 10-8 mm³/N-M
55.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK
LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
K (wear) Factor 111 x 10-8 mm³/N-M
55.0 x 10-10 in³-min/ft-lb-hr
ASTM D3702
Ensinger Delrin® 150 Homopolymer Acetal (POM)
Ensinger's Delrin® 150 stock shapes are a homopolymer acetal manufactured using DuPont Delrin 150 Resin. It is a crystalline plastic which offers an excellent balance of properties to bridge the g..