Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 967 x 10-8 mm³/N-M | 480 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP AI001XXH ABS LNP* Lubricomp* AI001XXH is a compound based on ABS containing 2% Silicone. Characteristics of this grade are: Healthcare and Internally Lubricated. |