Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 755 x 10-8 mm³/N-M | 375 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
K (wear) Factor | 755 x 10-8 mm³/N-M | 375 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet) KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. .. |
|||
K (wear) Factor | 755 x 10-8 mm³/N-M | 375 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet) |
|||
K (wear) Factor | 755 x 10-8 mm³/N-M | 375 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet) |
|||
K (wear) Factor | 755 x 10-8 mm³/N-M | 375 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Technetics Group Amicon™ PEEK
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
K (wear) Factor | 755 x 10-8 mm³/N-M | 375 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |