Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 70.0 - 302 x 10-8 mm³/N-M | 34.7 - 150 x 10-10 in³-min/ft-lb-hr | Average value: 184 x 10<sup>-8</sup> mm³/N-M Grade Count:3 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
K (wear) Factor | 70.0 x 10-8 mm³/N-M @Pressure 1.75 MPa |
34.7 x 10-10 in³-min/ft-lb-hr @Pressure 254 psi |
31.4 m/min |
Global EPP PA 6C WFN Cast Polyamide 6 + Wax Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
K (wear) Factor | 70.0 x 10-8 mm³/N-M | 34.7 x 10-10 in³-min/ft-lb-hr | |
LATI Latilub 66-01M PA66, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |