Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 50.4 x 10-8 mm³/N-M | 25.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
K (wear) Factor | 50.4 x 10-8 mm³/N-M | 25.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
K (wear) Factor | 50.4 x 10-8 mm³/N-M | 25.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT LNP* LUBRICOMP WL002 is a compound based on PBT resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
K (wear) Factor | 50.4 x 10-8 mm³/N-M | 25.0 x 10-10 in³-min/ft-lb-hr | Thrust washer at 2000 PV |
Techmer ES Plaslube® J-1/30/TF/10 Nylon 66, 30% GFR, 10% PTFE Plaslube glass fiber reinforced, polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer an excellent balance of wear and friction performance and mechanical strength. The addition of silic.. |
|||
K (wear) Factor | 50.4 x 10-8 mm³/N-M | 25.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
K (wear) Factor | 50.4 x 10-8 mm³/N-M | 25.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
K (wear) Factor | 50.4 x 10-8 mm³/N-M | 25.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
K (wear) Factor | 50.4 x 10-8 mm³/N-M | 25.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |