Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 4.30 x 10-8 mm³/N-M | 2.13 x 10-10 in³-min/ft-lb-hr | |
LATI Latilub 80-10T Y/15 PPS, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |