Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 318 x 10-8 mm³/N-M | 158 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC LNP LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
K (wear) Factor | 318 x 10-8 mm³/N-M | 158 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 318 x 10-8 mm³/N-M | 158 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific) LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |