Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 27.2 x 10-8 mm³/N-M | 13.5 x 10-10 in³-min/ft-lb-hr | Dry: 4 m/s, 0.2 MPa (800 fpm, 31.25 psi); ASTM D3702 |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h.. |