Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 1.00 - 5.00 x 10-8 mm³/N-M | 0.496 - 2.48 x 10-10 in³-min/ft-lb-hr | |
BACT DLC Diamond-Like Coating DLC (a-C:H). This coating provides the highest hardness and abrasion resistance of the BACT products. Typical applications include high wear environments involving seals, molds, metal forming, and.. |