Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 10.0 - 15.0 x 10-8 mm³/N-M | 4.96 - 7.45 x 10-10 in³-min/ft-lb-hr | at PV 100; ASTM D3702 |
Guarniflon PTFE G427 Polytetrafluoroethylene 40% Bronze, 5% Molybdenum Disulfide PTFE G Special Compound with bronze and molybdenum disulphiteInformation provided by Guarniflon® |
|||
K (wear) Factor | 10.0 - 15.0 x 10-8 mm³/N-M | 4.96 - 7.45 x 10-10 in³-min/ft-lb-hr | at PV 100; ASTM D3702 |
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |