Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 806 x 10-8 mm³/N-M | 400 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet) Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha.. |
|||
K (wear) Factor | 806 x 10-8 mm³/N-M | 400 x 10-10 in³-min/ft-lb-hr | QTM 55007 |
Quadrant EPP Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Broadest size range availability Good mechanical and electrical properties Ideal balance of strength and toughness Cast as finished parts and n.. |