Polymer Property : K (wear) Factor = 449 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 449 x 10-8 mm³/N-M
223 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubriloy DF202 PC
LNP LUBRILOY* DF202 is a compound based on Polycarbonate resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied b..
K (wear) Factor 449 x 10-8 mm³/N-M
223 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY DF202P PC
LNP LUBRILOY* DF202P is a compound based on Polycarbonate resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Exceptional Processing.